Series 270
Stranlok
Generic Type
Polyamine Epoxy
Common Usage
A high-performance, fiberglass-reinforced wall coating for protection against acids, alkalis and physical abuse. Stranlok’s 100% solids epoxy technology is solventless and VOC compliant, making Stranlok virtually odorless and permitting application in occupied facilities. Its accelerated curing schedule and installation process mean faster return-to-service times. A unique blend of two types of premixed reinforcing fibers allows Stranlok to be spray or trowel applied up to 40 mils. The integrity of the interlocking fibers allows the surface to withstand daily high-pressure steam cleaning. In addition to this high tolerance to “thermal shock,” Stranlok also features broad chemical, impact and abrasion resistance.
View more product detailsProduct Data Sheets
- English_Series_270_Stranlok_pds.pdf
- French_Series_270_Stranlok_pds.pdf
- Spanish_Series_270_Stranlok_pds.pdf
Safety Data Sheets
Email this productContact your sales reps for quotes, problem solving advice, extensive technical knowledge, pricing, ordering and field support.
Colors
View Available Colors
View available colors in our Color Tool; you can also select and request color swatches.
Recommended DFT
25 to 40 mils (635 to 1,015 microns) per coat.
Volume Solids
100% (mixed)
Surfacer/Filler/Patcher
CMU, Concrete & Cement Board: Series 130, 215, 218, 1254. Series 201 mixed with fumed silica (refer to Technical Bulletin 98-11). Refer to the applicable product data sheet for additional information. CMU or concrete must be filled or resurfaced with a recommended product prior to priming.
Curing Time
Temperature | To Topcoat | To Place in Service † |
---|---|---|
75°F (24°C) | 12-24 hours | 24 hours |
Note: If more than 24 hours have elapsed between coats, the coated surface must be mechanically abraded before topcoating. † Note: Severe service may require a longer curing time. Contact your Tnemec representative or Tnemec Technical Services. Curing time varies with surface temperature, air movement, humidity and film thickness.
Primers
Wood, Drywall & Pre-cast Concrete: Self-priming or Series 201, 233
CMU: Series 201 overfilled CMU
Note: For taping joints on wallboard or drywall, in areas that will be frequently wet, subject to chemical cleaning, thermal shock, impact, and VHP (or similar) cleaning, use Sheetrock brand Durabond 90. For taping joints on wood or cement board, use Series 273 Part D fiberglass tape and Series 215 as the taping compound. Reference Technical Bulletin 21-118.
Volatile Organic Compounds
Unthinned: 0.02 lbs/gallon (3 grams/litre)
Thinned 3% (No. 42 Thinner): 0.22 lbs/gallon (26 grams/litre)
Number of Components
Two: Part A (epoxy) and Part B (amine)
Theoretical Coverage
1,604 mil sq ft/gal (39.4 m²/L at 25 microns). See APPLICATION for coverage rates.
Topcoats
Series 22, 73, 113, 114, 280, 280FC, 282, 287, V290, 297, 1080, 1081. Note: Series 270 must be topcoated with 22, 280, 280FC, 282, or 287, prior to application of 73, 113, 114, V290, 297, 1080, or 1081 finish coats. Refer to the applicable product data sheet for color availability and additional information.
Still have questions? Request the information you’re looking for:
Request InfoHow to Purchase
Tnemec coatings are sold through a select network of local independent sales representatives who can help you find the best product for your needs. Find a rep